EUR
15,50
/per pcs.
incl. 20% VAT plus Shipping Cost. |
In stock.
| If an order includes hardening, we will wait to ship until the blade(s) have arrived and have been hardened. |
The material thickness at the edge must be at least 0,6 mm for carbon steel and 0,4 mm for stainless steel. For laminated steel, only grind down to 1 mm.
Maximum width of the blank: 100mm
Please clearly mark each blade and include a note with: address, order number, steel specification as well as which blade, if any, should be measured for individual HRC testing or the hardness certificate.
Note on the measuring point: For a correct Rockwell test, the measuring area must be metallically clean and flat. We therefore prepare the surface if necessary in the measuring area at the tang/handle transition by lightly removing scale or oxide layer. Measurements are only possible if the handle/tang provides enough area (min. 10x10mm) and does not have an excessively irregular thickness (e.g., with a forged tang).
The following is carried out during heat treatment:
Carbon steel is hardened in the furnace without scale protection, and the resulting scale is partially brushed off, especially on the blade. Stainless steel & PM steel are protected in an argon atmosphere and air-quenched, resulting in only a very thin oxide layer.
Rust-prone laminated steel (carbon steel) is not cryo treated due to the increased risk of cracking.
Blades must be sent in with a symmetrical grind and in compliance with our minimum edge thickness requirements. Blades ground thinner are particularly at risk of warping and distortion. Even with professional heat treatment and subsequent straightening, residual warping, cracks, or fractures may occur.
For further information, please visit our website.